<p>This is useful as a test of mastery of the preceding exercise. A piece of 3⁄16 or 7⁄32 inch tubing is joined to each end of a piece of tubing 5⁄8 by about 5 inches, and two constrictions made in the large tube, by the method described on page 10. The small tubes are then bent in the same plane, as shown, and their ends fire-polished (Fig. 9).<br>
<br>
</p>
<div> <img src="images/i036.png" alt="" title="" width="400" height="98"> Fig. 9.—Tube for condensing sulphur dioxide. <br>
<br>
</div>