Constricting A Tube

Where a constriction is to be made in a tube, the above method must be modified, as the strength of the tube must be maintained, and the constricted portion is usually short. Small tubes…

Where a constriction is to be made in a tube, the above method must be modified, as the strength of the tube must be maintained, and the constricted portion is usually short. Small tubes are often constricted without materially changing their outside diameter, by a process of thickening the walls. The tube is heated before the blast lamp, rotating it about its axis as later described, and as it softens is gradually pushed together so as to thicken the walls at the heated point, as in <em>a</em>, Fig. 1. When this operation has proceeded far enough, the tube is removed from the flame, and the ends cautiously and gently drawn apart, continuing the rotation of the tube about its axis and taking care not to draw too rapidly at first. The resulting tube should have a uniform exterior diameter, as shown in <em>b</em>, Fig. 1.</p>

<div> <img src="images/i018.png" alt="" title="" width="355" height="400"> Fig. 1.—Constricting a tube.<br>

<br>

</div>

<p>This method of constriction is not suited to tubes much over 1⁄4 inch in diameter, since the mass of glass in the constricted part becomes so thick as to be difficult to handle when hot, and likely to crack on cooling. Larger tubes are therefore constricted by heating in a narrow flame, with constant rotation, and when soft, alternately gently pulling the ends apart and pushing them together, each motion being so regulated that the diameter of a short section of the tube is gradually reduced, while the thickness of the wall of the reduced portion remains the same as that of the rest of the tube, or increases only slightly. This pulling and pushing of the glass takes place <em>in the flame</em>, while the rotation is being continued regularly. The result may appear as indicated in <em>c</em>, Fig. 1. The strength of the work depends upon the thickness of the walls of the constricted portion, which should never be less than that in the main tube, and usually a little greater. This operation is most successful with tubing having a relatively thin wall.</p>

Source

This piece is part of Laboratory Manual Of Glass-blowi. Explore the full collection for more from this work.

Previous Flanging A Tube Next Drawing Out A Tube